RangeNPS ½ to 24
Pressure, A105 at 38 °C68.1 bar
Standard raised face (RF)6.4 mm
TypesWN · SO · SW · TH · LJ · BL

Types and range in class 400

ASME B16.5 class 400 flange types and diameter range
TypeCodeRange
Weld neckWNNPS ½ to 24
Slip-onSONPS ½ to 24
Socket weldSWNPS ½ to 3
ThreadedTHNPS ½ to 24
Lap jointLJNPS ½ to 24
BlindBLNPS ½ to 24
Section of a weld neck flange with dimensions O, tf, R, W, X, Ah, Y and B ORWX tfYAhB pipe axis
Section of the weld neck (WN) flange. O outside diameter · tf thickness · R raised face · W bolt circle · X hub at base · Ah diameter at bevel · Y length · B bore.

Up to NPS 3½, ASME B16.5 requires class 400 to use the same dimensions as class 600. In the tables these rows appear with "= 600" next to the NPS.

General dimensions and weld neck (WN) flange

Class 400 flange: dimensions in mm, weight in kg (estimated*)
NPSDNOtfRXAhY WNB WNWN weight*Blind weight*
½" = 600159514.235.13821.352customer0.90.8
¾" = 6002011715.742.94826.757customer1.51.3
1" = 6002512417.550.85433.562customer1.81.6
1¼" = 6003213320.663.56442.267customer2.52.2
1½" = 6004015522.4737048.370customer3.53.3
2" = 6005016525.491.98460.573customer4.34.1
2½" = 6006519028.4104.610073.279customer6.36.1
3" = 6008021031.812711788.983customer8.58.5
3½" = 6009022935.1139.7133101.686customer10.711
4"10025435.1157.2146114.389customer13.313.8
5"12527938.1185.7178141.2102customer17.518.4
6"15031841.1215.9206168.4103customer22.925.5
8"20038147.8269.7260219.2117customer36.142.8
10"25044453.8323.8321273.0124customer50.464.2
12"30052157.2381375323.8137customer72.694.6
14"35058460.5412.8425355.6149customer99.7124.8
16"40064863.5469.9483406.4152customer123.4161.7
18"45071166.5533.4533457.2165customer150.5204.2
20"50077569.8584.2587508.0168customer179.1254.3
22"55083873.2641.4641558.8171customer210.5311.8
24"60091476.2692.2702609.6175customer258.2385.8

Slip-on, socket weld, threaded and lap joint

Class 400 flange: lengths and bores by type, in mm
NPS Y SO / SW / TH B SO / SW D socket T threadQ counterbore Y LJB LJr LJ SO weight*
½" = 600 2222.410 1623.6 2222.93 0.7
¾" = 600 2527.711 1629.0 2528.23 1.2
1" = 600 2734.513 1835.8 2735.13 1.5
1¼" = 600 2843.214 2144.4 2843.75 2
1½" = 600 3249.516 2250.5 3250.06 3
2" = 600 3762.018 2863.5 3762.58 3.6
2½" = 600 4174.719 3276.2 4175.48 5.2
3" = 600 4690.721 3592.2 4691.410 7
3½" = 600 49103.4– 40104.9 49104.110 8.8
4" 51116.1– 37117.6 51116.811 11.1
5" 54143.8– 43144.5 54144.511 13.8
6" 57170.7– 46171.4 57171.413 18.2
8" 68221.5– 51222.2 68222.213 28.5
10" 73276.4– 56276.4 102277.413 38.8
12" 79327.2– 60328.7 108328.213 56.8
14" 84359.2– 64360.4 117360.213 78.7
16" 94410.5– 68411.2 127411.213 100.6
18" 99461.8– 70462.0 137462.313 121.7
20" 102513.1– 73512.8 146514.413 145.9
22" 108564.4– –– 152565.213 174.1
24" 114616.0– 83614.4 159616.013 217.5

Y = overall length without raised face · B = minimum bore · D = socket depth · T = minimum thread length · Q = thread counterbore diameter · r = lap joint bore radius. "–" = type not covered by the standard at this diameter.

Bolt pattern and bolting

Class 400 flange: bolt pattern (mm) and bolts (in)
NPSOW (bolt circle)No. of holesHole ØBolt ØStud bolt, RFStud bolt, RTJ
½" = 6009566.54⅝"½"7575
¾" = 60011782.64¾"⅝"9090
1" = 60012488.94¾"⅝"9090
1¼" = 60013398.64¾"⅝"9595
1½" = 600155114.34⅞"¾"110110
2" = 600165127.08¾"⅝"110110
2½" = 600190149.48⅞"¾"120120
3" = 600210168.18⅞"¾"125125
3½" = 600229184.281"⅞"140140
4"254200.281"⅞"140140
5"279235.081"⅞"145145
6"318269.7121"⅞"150150
8"381330.2121⅛"1"170170
10"444387.4161¼"1⅛"190190
12"521450.8161⅜"1¼"205205
14"584514.4201⅜"1¼"210210
16"648571.5201½"1⅜"220220
18"711628.6241½"1⅜"230230
20"775685.8241⅝"1½"240250
22"838743.0241¾"1⅝"255260
24"914812.8241⅞"1¾"265280

Stud bolt length in mm, excluding the ends. Ring type joints (RTJ) use a longer stud in almost all diameters.

Allowable pressure of class 400 (bar)

Working pressure of class 400 by material group and temperature
Material (group)−29 to 38 °C100 °C200 °C300 °C400 °C
Carbon steel A105 / A350 LF2 (1.1)68.162.158.453.146.3
Stainless F304 / F304H (2.1)66.254.546.041.237.9
Stainless F316 / F316H (2.2)66.256.347.642.239.3
Duplex F51, super duplex F53 / F55 (up to 315 °C), 6Mo F44 (2.8)68.967.556.951.848.9
Inconel 625, Incoloy 825, Hastelloy C-276 / C-22 (3.8)68.968.764.557.048.9

Values from ASME B16.5 tables 2-1.1 to 2-3.8. "–" = material outside the standard's temperature range. For other groups and temperatures, consult engineering.

Table notes

  • Dimensions without the raised face: add 6.4 mm to the thickness (tf) and length (Y) of raised-face flanges.
  • "= 600" next to the NPS: up to NPS 3½, class 400 uses the same dimensions as class 600, as the standard requires.
  • * Weight estimated from geometry in carbon steel, with STD bore when the customer does not state the schedule. Stainless weighs about 1 % more; nickel alloys 7 % to 13 % more.
  • "customer" = the WN bore follows the pipe schedule stated in the order.

Frequently asked questions

What does class 400 flange (400#, 400 lb) mean?

It is the ASME B16.5 pressure class. It is not the pressure in psi: it defines an allowable pressure vs. temperature curve for each material group. In A105 carbon steel, class 400 allows 68.1 bar from −29 to 38 °C and less as the temperature rises.

Which flange types exist in class 400?

Weld neck (WN): NPS ½ to 24; Slip-on (SO): NPS ½ to 24; Socket weld (SW): NPS ½ to 3; Threaded (TH): NPS ½ to 24; Lap joint (LJ): NPS ½ to 24; Blind (BL): NPS ½ to 24.

Do the thickness (tf) and length (Y) include the raised face?

No. Since the 2017 edition, tf and Y are measured without the raised face. In class 400 the standard raised face is 6.4 mm, which is added to the table thickness.

What is the bore (B) of the weld neck flange?

The WN bore follows the pipe wall thickness (schedule). The standard gives the standard-wall (STD) bore only for classes 150 and 300 up to NPS 12; in the other cases the customer states the schedule in the order.

Class 400 flange in any alloyA105, F316L, F51, F53/F55, F22, Inconel 625 and others, forged and machined at Dustre, with 3.1 certificate.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)