ASME B16.47 Series B class 75 flange: dimensions and bolt pattern

Large-diameter flanges, NPS 26 to 60, weld neck (WN) and blind. Series B (formerly API 605) has more compact and lighter flanges, with more, smaller-diameter bolts. Common in heat exchangers and equipment.

Technical review Oct 2026 · Source: ASME B16.47

RangeNPS 26 to 60
Pressure, A105 at 38 °Cper standard
TypesWeld neck (WN) and blind
SeriesB (ex-API 605)

Dimensions and bolt pattern

B16.47 Series B class 75 flange: dimensions in mm, bolts in inches, weight in kg (estimated)
NPSDNOtf WNtf blindXAhYWHolesHole ØBoltWN weight*Blind weight*
26"650762.031.831.8676.1661.957.1723.93619.1⅝"36111
28"700812.831.831.8726.9712.760.5774.74019.1⅝"39127
30"750863.631.831.8777.7763.563.5825.54419.1⅝"42143
32"800914.433.533.8828.5814.368.3876.34819.1⅝"48171
34"850965.233.536.6879.3865.171.6927.15219.1⅝"51206
36"9001033.535.140.9935.0915.984.3992.14022.2¾"69264
38"9501084.336.642.9985.8965.287.41042.94022.2¾"77306
40"10001135.136.642.91036.61017.590.71093.74422.2¾"80335
42"10501185.938.146.21087.41068.393.71144.54822.2¾"87394
44"11001251.041.447.81139.21119.1103.41203.53625.4⅞"109454
46"11501301.842.949.31190.81169.9106.41254.34025.4⅞"118507
48"12001352.644.552.61240.31220.7109.71305.14425.4⅞"126584
50"12501403.446.254.11293.91271.5114.31355.94425.4⅞"138647
52"13001457.546.255.61344.71322.3119.11409.74825.4⅞"148718
54"13501508.347.858.91397.01373.1124.01460.54825.4⅞"161815
56"14001574.849.360.51450.81423.9133.31521.04028.61"192913
58"14501625.650.862.01501.61474.7136.71571.84428.61"203996
60"15001676.454.165.31552.41525.5143.01609.94428.61"2231117

O = outside diameter · tf = thickness (without raised face) · X = hub at base · Ah = diameter at bevel · Y = overall length of the WN · W = bolt circle. Weight estimated in carbon steel with STD wall bore; stainless ≈ +1 %, nickel alloys +7 % to +13 %.

Frequently asked questions

What is the difference between Series A and Series B of ASME B16.47?

Both cover NPS 26 to 60, but they are not interchangeable: outside diameter, bolt circle and number of bolts are different. Series A is more robust (formerly MSS SP-44); Series B is more compact (formerly API 605). Check the series on the drawing before buying.

When to use ASME B16.47 instead of B16.5?

ASME B16.5 goes up to NPS 24. From NPS 26 to 60, ASME B16.47 applies, in Series A or B.

B16.47 flange made to orderForged and machined at Dustre in carbon steel, stainless, duplex and nickel alloys, with 3.1 certificate.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)