ASME B16.47 B 系列 75 级法兰:尺寸和螺栓孔布置

大口径法兰,NPS 26 至 60,对焊 (WN) 和盲板。 B 系列(原 API 605)法兰更紧凑、更轻,螺栓数量多、直径小,常见于换热器和设备。

技术审核 2026年10月 · 来源: ASME B16.47

规格范围NPS 26 至 60
压力,A105 材料 38 °C 时按标准
类型对焊 (WN) 和盲板
系列B (ex-API 605)

尺寸与螺栓孔布置

B16.47 B 系列 75 级法兰:尺寸(毫米)、螺栓(英寸)、重量(千克,估算)
NPSDNOtf WN盲板 tfXAhYW孔孔 Ø螺栓WN 重量*盲板重量*
26"650762.031.831.8676.1661.957.1723.93619.1⅝"36111
28"700812.831.831.8726.9712.760.5774.74019.1⅝"39127
30"750863.631.831.8777.7763.563.5825.54419.1⅝"42143
32"800914.433.533.8828.5814.368.3876.34819.1⅝"48171
34"850965.233.536.6879.3865.171.6927.15219.1⅝"51206
36"9001033.535.140.9935.0915.984.3992.14022.2¾"69264
38"9501084.336.642.9985.8965.287.41042.94022.2¾"77306
40"10001135.136.642.91036.61017.590.71093.74422.2¾"80335
42"10501185.938.146.21087.41068.393.71144.54822.2¾"87394
44"11001251.041.447.81139.21119.1103.41203.53625.4⅞"109454
46"11501301.842.949.31190.81169.9106.41254.34025.4⅞"118507
48"12001352.644.552.61240.31220.7109.71305.14425.4⅞"126584
50"12501403.446.254.11293.91271.5114.31355.94425.4⅞"138647
52"13001457.546.255.61344.71322.3119.11409.74825.4⅞"148718
54"13501508.347.858.91397.01373.1124.01460.54825.4⅞"161815
56"14001574.849.360.51450.81423.9133.31521.04028.61"192913
58"14501625.650.862.01501.61474.7136.71571.84428.61"203996
60"15001676.454.165.31552.41525.5143.01609.94428.61"2231117

O = 外径 · tf = 厚度(不含凸台)· X = 根部颈部直径 · Ah = 坡口处直径 · Y = WN 总长 · W = 螺栓孔中心圆。重量按碳钢 STD 壁厚内径估算;不锈钢约 +1 %,镍基合金 +7 % 至 +13 %。

常见问题

ASME B16.47 的 A 系列和 B 系列有什么区别?

两者都覆盖 NPS 26 至 60,但不能互换:外径、螺栓孔中心圆和螺栓数量均不同。A 系列更坚固(原 MSS SP-44);B 系列更紧凑(原 API 605)。购买前请对照图纸确认系列。

什么时候用 ASME B16.47 而不是 B16.5?

ASME B16.5 最大到 NPS 24。NPS 26 至 60 适用 ASME B16.47,分 A 系列或 B 系列。

按订单制造的 B16.47 法兰由 Dustre 锻造并机加工,材料有碳钢、不锈钢、双相钢和镍基合金,附 3.1 证书。
申请报价
Helena虚拟助理 · WhatsApp

申请报价

主题: . 填写并发送:您的请求将转给我们的技术团队,我们会通过电子邮件回复。

更多信息(可选):税号、交货地、期限和要求
要求

图纸、清单或规格。最多 5 个文件,总计 15 MB。

通过 WhatsApp 发送

我们仅将您的数据用于答复本次报价。 隐私. · WhatsApp +55 11 98649-0075 · 周一至周四 07:00–17:00 · 周五 07:00–16:00(巴西利亚时间)