Dustre
EN
Customer area

ASME B16.47 Series B class 150 flange: dimensions and bolt pattern

Large-diameter flanges, NPS 26 to 60, weld neck (WN) and blind. Series B (formerly API 605) has more compact and lighter flanges, with more, smaller-diameter bolts. Common in heat exchangers and equipment.

Technical review Oct 2026 · Source: ASME B16.47

RangeNPS 26 to 60
Pressure, A105 at 38 °C19.6 bar
TypesWeld neck (WN) and blind
SeriesB (ex-API 605)

Dimensions and bolt pattern

B16.47 Series B class 150 flange: dimensions in mm, bolts in inches, weight in kg (estimated)
NPSDNOtf WNtf blindXAhYWHolesHole ØBoltWN weight*Blind weight*
26"650785.939.942.9684.3661.987.4744.53622.2¾"58159
28"700836.742.946.2735.1712.793.7795.34022.2¾"66194
30"750887.542.949.3787.4763.598.6846.14422.2¾"72233
32"800941.344.552.6839.7814.3106.4900.24822.2¾"83280
34"8501004.847.855.6892.0865.1108.7957.34025.4⅞"100337
36"9001057.150.857.1944.6915.9116.11009.74425.4⅞"114383
38"9501124.052.662.0997.0968.2122.41069.84028.61"135470
40"10001174.854.165.31049.31019.0127.01120.64428.61"146541
42"10501225.657.166.81101.91069.8131.81171.44828.61"161602
44"11001276.458.969.91152.71120.6135.11222.25228.61"172684
46"11501341.460.573.21205.01171.4143.01284.24031.81⅛"203794
48"12001392.263.576.21257.31222.2147.81335.04431.81⅛"205890
50"12501443.066.879.51308.11273.0152.41385.84831.81⅛"239997
52"13001493.868.382.51360.41323.8155.71436.65231.81⅛"2541108
54"13501549.469.985.91412.71371.6160.51492.35631.81⅛"2831241
56"14001600.271.688.91465.31425.4165.11543.16031.81⅛"2951370
58"14501674.973.291.91516.11476.2173.21611.44834.91¼"3531556
60"15001725.774.795.31570.01527.0177.81662.25234.91¼"3741713

O = outside diameter · tf = thickness (without raised face) · X = hub at base · Ah = diameter at bevel · Y = overall length of the WN · W = bolt circle. Weight estimated in carbon steel with STD wall bore; stainless ≈ +1 %, nickel alloys +7 % to +13 %.

Allowable pressure of class 150 (bar)

Working pressure of class 150 by material group and temperature
Material (group)−29 to 38 °C100 °C200 °C300 °C400 °C
Carbon steel A105 / A350 LF2 (1.1)19.617.713.810.26.5
Stainless F304 / F304H (2.1)19.015.713.210.26.5
Stainless F316 / F316H (2.2)19.016.213.710.26.5
Duplex F51, super duplex F53 / F55 (up to 315 °C), 6Mo F44 (2.8)20.017.713.810.26.5
Inconel 625, Incoloy 825, Hastelloy C-276 / C-22 (3.8)20.017.713.810.26.5

ASME B16.47 uses the same pressure classes as B16.5. "–" = material outside the temperature range.

Frequently asked questions

What is the difference between Series A and Series B of ASME B16.47?

Both cover NPS 26 to 60, but they are not interchangeable: outside diameter, bolt circle and number of bolts are different. Series A is more robust (formerly MSS SP-44); Series B is more compact (formerly API 605). Check the series on the drawing before buying.

When to use ASME B16.47 instead of B16.5?

ASME B16.5 goes up to NPS 24. From NPS 26 to 60, ASME B16.47 applies, in Series A or B.

What is the pressure of a B16.47 class 150 flange?

The pressure class follows the same tables as ASME B16.5. In A105 carbon steel, class 150 allows 19.6 bar from −29 to 38 °C.

B16.47 flange made to orderForged and machined at Dustre in carbon steel, stainless, duplex and nickel alloys, with 3.1 certificate.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)