ASME B16.47 Series A class 150 flange: dimensions and bolt pattern

Large-diameter flanges, NPS 26 to 60, weld neck (WN) and blind. Series A (formerly MSS SP-44) has more robust flanges, with fewer, larger-diameter bolts. It is the most used in process piping.

Technical review Oct 2026 · Source: ASME B16.47 · * corrected value or to be confirmed

RangeNPS 26 to 60
Pressure, A105 at 38 °C19.6 bar
TypesWeld neck (WN) and blind
SeriesA (ex-MSS SP-44)

Dimensions and bolt pattern

B16.47 Series A class 150 flange: dimensions in mm, bolts in inches, weight in kg (estimated)
NPSDNOtf WNtf blindXAhYWHolesHole ØBoltWN weight*Blind weight*
26"650870.066.866.8676.1660.4119.1806.52434.91¼"142300
28"700927.169.969.9726.9711.2124.0863.62834.91¼"162356
30"750984.373.273.2781.1762.0*135.1914.4*2834.91¼"189422
32"8001060.579.579.5831.9812.8*143.0977.9*2841.31½"237528
34"8501111.381.081.0882.6863.6*147.81028.7*3241.31½"253589
36"9001168.488.988.9933.5914.4155.71085.83241.31½"300718
38"9501238.385.985.9990.6965.2155.71149.43241.31½"335783
40"10001289.188.988.91041.41016.0162.11200.23641.31½"361877
42"10501346.295.395.31092.21066.8169.91257.33641.31½"4151029
44"11001403.4100.1100.11143.01117.6176.31314.54041.31½"4621173
46"11501454.2101.6101.61196.81168.4184.21365.34041.31½"4941282
48"12001511.3106.4106.41247.61219.2190.51422.44441.31½"5461449
50"12501568.5109.7109.71301.81270.0201.71479.64447.61¾"5881597
52"13001625.6114.3114.31351.31320.8208.01536.74447.61¾"6501792
54"13501682.8119.1119.11403.41371.6214.41593.94447.61¾"7192006
56"14001746.3122.4122.41457.51422.4227.11651.04847.61¾"8002219
58"14501803.4127.0127.01508.31473.2233.41708.24847.61¾"8762461
60"15001854.2130.3130.31559.11524.0238.31759.05247.61¾"9222667

O = outside diameter · tf = thickness (without raised face) · X = hub at base · Ah = diameter at bevel · Y = overall length of the WN · W = bolt circle. Weight estimated in carbon steel with STD wall bore; stainless ≈ +1 %, nickel alloys +7 % to +13 %.

Allowable pressure of class 150 (bar)

Working pressure of class 150 by material group and temperature
Material (group)−29 to 38 °C100 °C200 °C300 °C400 °C
Carbon steel A105 / A350 LF2 (1.1)19.617.713.810.26.5
Stainless F304 / F304H (2.1)19.015.713.210.26.5
Stainless F316 / F316H (2.2)19.016.213.710.26.5
Duplex F51, super duplex F53 / F55 (up to 315 °C), 6Mo F44 (2.8)20.017.713.810.26.5
Inconel 625, Incoloy 825, Hastelloy C-276 / C-22 (3.8)20.017.713.810.26.5

ASME B16.47 uses the same pressure classes as B16.5. "–" = material outside the temperature range.

Frequently asked questions

What is the difference between Series A and Series B of ASME B16.47?

Both cover NPS 26 to 60, but they are not interchangeable: outside diameter, bolt circle and number of bolts are different. Series A is more robust (formerly MSS SP-44); Series B is more compact (formerly API 605). Check the series on the drawing before buying.

When to use ASME B16.47 instead of B16.5?

ASME B16.5 goes up to NPS 24. From NPS 26 to 60, ASME B16.47 applies, in Series A or B.

What is the pressure of a B16.47 class 150 flange?

The pressure class follows the same tables as ASME B16.5. In A105 carbon steel, class 150 allows 19.6 bar from −29 to 38 °C.

B16.47 flange made to orderForged and machined at Dustre in carbon steel, stainless, duplex and nickel alloys, with 3.1 certificate.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)