ASME B16.47 Series A class 900 flange: dimensions and bolt pattern

Large-diameter flanges, NPS 26 to 48, weld neck (WN) and blind. Series A (formerly MSS SP-44) has more robust flanges, with fewer, larger-diameter bolts. It is the most used in process piping.

Technical review Oct 2026 · Source: ASME B16.47 · * corrected value or to be confirmed

RangeNPS 26 to 48
Pressure, A105 at 38 °C153.2 bar
TypesWeld neck (WN) and blind
SeriesA (ex-MSS SP-44)

Dimensions and bolt pattern

B16.47 Series A class 900 flange: dimensions in mm, bolts in inches, weight in kg (estimated)
NPSDNOtf WNtf blindXAhYWHolesHole ØBoltWN weight*Blind weight*
26"6501085.8139.7160.3774.7660.4285.8952.52073.02¾"6641060
28"7001168.4142.7171.5831.9711.2298.41022.42076.22⅞"7901321
30"7501231.9149.4182.4889.0762.0311.21085.82076.22⅞"9131576
32"8001314.5158.8193.5946.1812.8330.21155.72085.73¼"10841886
34"8501397.0165.1204.71006.3863.6349.31225.62092.13½"12722249
36"9001460.5171.5214.41063.8914.4361.91289.12092.13½"14382595
38"9501460.5190.5215.91073.2965.2352.61289.12092.13½"13992614
40"10001511.3196.8223.81127.31016.0363.51339.92492.13½"14782871
42"10501562.1206.2*231.61176.31066.8371.31390.72492.13½"16123194
44"11001648.0214.4242.81234.91117.6390.71463.52498.43¾"18813718
46"11501733.6225.6255.51292.41168.4411.01536.724104.84"21984319
48"12001784.4233.4263.71343.21219.2419.11587.524104.84"23624748

O = outside diameter · tf = thickness (without raised face) · X = hub at base · Ah = diameter at bevel · Y = overall length of the WN · W = bolt circle. Weight estimated in carbon steel with STD wall bore; stainless ≈ +1 %, nickel alloys +7 % to +13 %.

Allowable pressure of class 900 (bar)

Working pressure of class 900 by material group and temperature
Material (group)−29 to 38 °C100 °C200 °C300 °C400 °C
Carbon steel A105 / A350 LF2 (1.1)153.2139.8131.4119.5104.2
Stainless F304 / F304H (2.1)148.9122.6103.492.785.3
Stainless F316 / F316H (2.2)148.9126.6107.094.988.3
Duplex F51, super duplex F53 / F55 (up to 315 °C), 6Mo F44 (2.8)155.1152.0128.0116.6109.8
Inconel 625, Incoloy 825, Hastelloy C-276 / C-22 (3.8)155.1154.6145.0128.6109.8

ASME B16.47 uses the same pressure classes as B16.5. "–" = material outside the temperature range.

Frequently asked questions

What is the difference between Series A and Series B of ASME B16.47?

Both cover NPS 26 to 60, but they are not interchangeable: outside diameter, bolt circle and number of bolts are different. Series A is more robust (formerly MSS SP-44); Series B is more compact (formerly API 605). Check the series on the drawing before buying.

When to use ASME B16.47 instead of B16.5?

ASME B16.5 goes up to NPS 24. From NPS 26 to 60, ASME B16.47 applies, in Series A or B.

What is the pressure of a B16.47 class 900 flange?

The pressure class follows the same tables as ASME B16.5. In A105 carbon steel, class 900 allows 153.2 bar from −29 to 38 °C.

B16.47 flange made to orderForged and machined at Dustre in carbon steel, stainless, duplex and nickel alloys, with 3.1 certificate.
Request a quote
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)