Aging

Aging forms fine precipitates that increase the strength of PH alloys. The temperature selects the combination of strength and toughness (H900, H1025, H1150).

Content reviewed by the Dustre technical team in Oct 2026

What we do

  • 17-4PH, 15-5PH, 17-7PH, Inconel 718, Monel K-500, A-286
  • Furnaces with temperature and time control and recording
  • Forgings, bars, blocks and machined parts
  • Report with the cycle applied and, on request, mechanical tests after treatment
Heat treatment furnace with computerized control
Illustrative photo: S zillayali, CC BY 3.0 (credits)

Materials

Austenitic, duplex and super duplex stainlessNickel alloys and titaniumCarbon, Cr-Mo and alloy steels

Capacity, maximum dimensions and lead time on request: send the drawing. See alloys in stock.

How aging works

After solution annealing, the alloy is held at an intermediate temperature for a few hours. During that time very fine precipitates form (copper in 17-4PH and 15-5PH, nickel-niobium in Inconel 718, nickel-aluminum-titanium in Monel K-500 and A-286) that block dislocation movement and raise the strength, without the distortion of a quench.

The H900 to H1150 conditions

In PH steels the condition is designated by the temperature in °F: H900 gives the highest strength and the lowest toughness; H1025, H1075 and H1150 trade strength for toughness and resistance to stress corrosion cracking. For H₂S service, NACE MR0175 limits 17-4PH to the double-aged conditions (H1150D) with a defined maximum hardness. Inconel 718 has different cycles for aerospace and for oil and gas (API 6ACRA).

Machining before or after

Aging distortion is small, so many parts are machined in the solution-annealed condition and aged afterwards. For tight tolerances we leave a minimum allowance for a final finishing cut after aging.

What to send with a quote request

To get a quote, send the alloy and standard of the material, the drawing or the dimensions of the part, the quantity, the required cycle (or the hardness and properties to be reached) and whether verification tests are needed. Parts that will still be machined are treated with allowance, so that the oxidized layer is removed in finish machining.

More in heat treatment

Related services

Frequently asked questions

Which aging condition should I choose?

By the combination of strength, toughness and service medium. H900 for maximum strength; H1025 or H1150 when there is impact or a risk of stress corrosion cracking; H1150D for H₂S service.

Does Dustre perform this service on customer-supplied material?

Yes, as long as the alloy and the specification are defined. We can also supply the material from our stock, with EN 10204 3.1 certificate.

Quote this serviceSend the drawing, alloy, quantity and standard. We reply with process, lead time and price.
Request a quoteWhatsApp
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)