Heat treatment

Stress relief

Stress relief reheats the part below the transformation temperature to reduce the stresses left by welding, forging or heavy machining.

Content reviewed by the Dustre technical team in Oct 2026

What we do

  • Post-weld heat treatment (PWHT) of fabricated and welded parts
  • Furnaces with temperature and time control and recording
  • Forgings, bars, blocks and machined parts
  • Report with the cycle applied and, on request, mechanical tests after treatment
Local heat treatment equipment for stress relief
Illustrative photo: CEphoto, Uwe Aranas, CC BY-SA 3.0 (credits)

Materials

Austenitic, duplex and super duplex stainlessNickel alloys and titaniumCarbon, Cr-Mo and alloy steels

Capacity, maximum dimensions and lead time on request: send the drawing. See alloys in stock.

How stress relief works

The part is heated below the transformation temperature (or, for non-hardenable alloys, below the recrystallization range), held until the temperature equalizes across the section and cooled slowly and in a controlled way. The heat lets the material yield locally and redistribute residual stresses, without significantly changing hardness and strength.

When it is required

Codes such as ASME Section VIII and B31.3 require post-weld heat treatment (PWHT) above certain thicknesses and for certain materials, such as Cr-Mo steels. Outside the code, stress relief is used before final machining of welded or heavily rough-machined parts, so the part does not distort after finishing, and on parts subject to stress corrosion cracking.

Precautions by alloy

The temperature changes a lot from one material to another. Carbon and Cr-Mo steels have ranges defined by the code; quenched and tempered steels must stay below the tempering temperature to avoid losing strength; austenitic stainless and duplex require care to avoid the sensitization and sigma phase ranges.

What to send with a quote request

To get a quote, send the alloy and standard of the material, the drawing or the dimensions of the part, the quantity, the required cycle (or the hardness and properties to be reached) and whether verification tests are needed. Parts that will still be machined are treated with allowance, so that the oxidized layer is removed in finish machining.

More in heat treatment

Related services

Frequently asked questions

Does stress relief reduce the hardness of the weld?

In Cr-Mo and carbon steels, yes: PWHT reduces the hardness of the heat-affected zone and the weld, which is precisely one of its goals. In quenched parts, the temperature is chosen so as not to reduce the hardness of the base metal.

Does Dustre perform this service on customer-supplied material?

Yes, as long as the alloy and the specification are defined. We can also supply the material from our stock, with EN 10204 3.1 certificate.

Quote this serviceSend the drawing, alloy, quantity and standard. We reply with process, lead time and price.
Request a quoteWhatsApp
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)