Dustre
EN
Customer area

Metal fabrication, forming and welding

Forming

Forming is shaping the metal without removing material. At Dustre this includes hot forging, bending and rolling of plates.

Content reviewed by the Dustre technical team in Oct 2026

What we do

  • Open-die hot forging
  • Plate bending on a press brake
  • Rolling of plates and sections
Hot rolling of a bar on a small rolling mill
Illustrative photo: Alan Murray-Rust, CC BY-SA 2.0 (credits)

Materials

Austenitic, duplex and super duplex stainlessNickel alloys and titaniumCarbon, Cr-Mo and alloy steels

Capacity, maximum dimensions and lead time on request: send the drawing. See alloys in stock.

Calculate the weight of bars, plates, pipes and blocks in any alloy →

What metal forming is

Forming is the set of processes that change the shape of the metal by plastic deformation, without removing material. At Dustre this includes open-die hot forging, plate bending on a press brake and rolling of plates and sections. Other forming processes, such as rolling, drawing and extrusion, are performed at the mills that produce the bars and plates in our stock.

Hot or cold

In hot forming, above the recrystallization temperature, the metal deforms with little force and does not work-harden; this is the case of forging. In cold forming, such as bending and rolling, the material work-hardens and becomes stronger and less ductile. Austenitic stainless and nickel alloys work-harden a lot: tight bends and severe rolling may require solution annealing afterwards, to restore ductility and corrosion resistance.

Choosing the process

Solid, thick-section parts are forged; plate parts are bent or rolled and then welded. We recommend the lowest-cost route for the geometry and alloy of the part.

What to send with a quote request

Send the drawing, the alloy, the thickness or section of the material, the quantity and the required final condition (formed, heat treated, machined).

More in metal fabrication, forming and welding

Related services

Frequently asked questions

Does cold forming make stainless magnetic?

It can, slightly. Austenitic stainless such as 304 and 316 forms a little martensite when heavily cold worked, and the part starts to attract a magnet in the bent regions. This does not indicate the wrong material, and solution annealing removes the effect.

Does Dustre perform this service on customer-supplied material?

Yes, as long as the alloy and the specification are defined. We can also supply the material from our stock, with EN 10204 3.1 certificate.

Quote this serviceSend the drawing, alloy, quantity and standard. We reply with process, lead time and price.
Request a quoteWhatsApp
HelenaVirtual assistant · WhatsApp

Request a quote

Subject: . Fill in and send: your request goes to our technical team and we reply by email.

More details (optional): tax ID, delivery, deadline and requirements
Requirements

Drawing, list or specification. Up to 5 files and 15 MB in total.

Send via WhatsApp

We use your data only to answer this quote. Privacy. · WhatsApp +55 11 98649-0075 · Mon–Thu 07:00–17:00 · Fri 07:00–16:00 (Brasília time)